Project Background
Chilean copper producer required an 800 TPD flotation concentrator for sulfide ore from a high-altitude Andean mine.
Process Design
Complete circuit: crushing → ball milling → rougher flotation → scavenger → two-stage cleaner with regrind. Automated reagent dosing and pH control.
Results
28.4% Cu concentrate grade at 91.8% recovery. Modular design enabled fast erection in 4.5 months.