Vanadium Extraction

Titanomagnetite deposits containing 0.5-1.5% V₂O₅ processed to extract vanadium.

Salt Roasting

Concentrate mixed with NaCl roasted at 800-850°C converts vanadium oxides to water-soluble sodium vanadate.

V₂O₅ Production

Purified vanadium solution precipitated as ammonium polyvanadate, calcined to produce V₂O₅ (98-99%) for steel alloying.